Fritte M2

OxideAnalysisFormula
CaO0.43%0.484
K2O0.12%0.082
Na2O0.43%0.435
Al2O30.21%0.128
B2O30.73%0.651
SiO22.67%2.754
Oxide Weight285.64
Formula Weight285.64
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 855C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fritte M2" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.439" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.125" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.436" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.211" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="0.733" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="2.679" tolerance=""/> </oxides> </material>