Fritte M1511

OxideAnalysisFormula
Na2O0.50%0.783
PbO0.50%0.217
B2O31.00%1.394
SiO21.50%2.422
Oxide Weight339.65
Formula Weight339.65
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 504C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Fritte M1511" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.500" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="0.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="1.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="1.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved