Frit Welte FR 2020

Lead bisilicate monoborate frit

Formula: PbO.B2O3.2SiO2

OxideAnalysisFormula
PbO54.04%1.000
B2O316.85%1.000
SiO229.10%2.000
Oxide Weight412.99
Formula Weight412.99
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit Welte FR 2020" descrip="Lead bisilicate monoborate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="54.040" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="16.850" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="29.100" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved