Frit Welte FR 2015

Lead bisilicate frit

Formula: PbO.2SiO2

OxideAnalysisFormula
PbO60.02%1.000
Al2O36.86%0.250
SiO233.13%2.050
Oxide Weight371.91
Formula Weight371.91
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 52.2 x10-7 (20-400C)
GTTM - Glass Transition Temperature 565C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit Welte FR 2015" descrip="Lead bisilicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="60.020" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.860" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="33.130" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved