Frit VO 6270

Reimbold & Strick stoneware tableware frit < 1050C

OxideAnalysisFormula
BaO4.00%0.076
K2O2.00%0.062
Na2O3.00%0.141
ZnO10.00%0.357
SrO13.00%0.365
B2O325.00%1.044
SiO243.00%2.080
Oxide Weight290.66
Formula Weight290.66
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 54 x 10-7 (20-400C)
GSPT - Frit Softening Point 660C
GTTM - Glass Transition Temperature 600C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit VO 6270" descrip="Reimbold & Strick stoneware tableware frit < 1050C" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="4.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="10.000" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="13.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="25.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="43.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved