Frit VO 6259

Reimbold & Strick stoneware tableware frit > 1050

OxideAnalysisFormula
BaO7.00%0.092
CaO15.00%0.540
MgO1.00%0.050
K2O2.00%0.043
Na2O1.00%0.033
ZnO9.00%0.223
SrO1.00%0.019
Al2O39.00%0.178
B2O34.00%0.116
SiO251.00%1.713
Oxide Weight201.84
Formula Weight201.84
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 60 x 10-7 (20-400C)
GSPT - Frit Softening Point 730C
GTTM - Glass Transition Temperature 670C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit VO 6259" descrip="Reimbold & Strick stoneware tableware frit > 1050" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="7.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="15.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="9.000" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="1.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved