Frit VO 6257

Reimbold & Strick fast double firing opaque frit

OxideAnalysisFormula
CaO10.00%0.387
MgO2.00%0.108
K2O6.00%0.138
ZnO13.00%0.347
PbO2.00%0.019
Al2O35.00%0.107
B2O310.00%0.312
SiO242.00%1.518
ZrO210.00%0.176
Oxide Weight217.28
Formula Weight217.28
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 65 x 10-7 (20-400C)
GSPT - Frit Softening Point 720C
GTTM - Glass Transition Temperature 610C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit VO 6257" descrip="Reimbold & Strick fast double firing opaque frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="6.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="13.000" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="2.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="10.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="42.000" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="10.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved