Frit VO 6255

Reimbold & Strick fast firing opaque frit

OxideAnalysisFormula
CaO11.00%0.426
MgO3.00%0.162
K2O4.00%0.092
ZnO12.00%0.320
Al2O34.00%0.085
B2O34.00%0.125
SiO253.00%1.915
ZrO29.00%0.159
Oxide Weight217.20
Formula Weight217.20
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 63 x 10-7 (20-400C)
GSPT - Frit Softening Point 700C
GTTM - Glass Transition Temperature 630C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit VO 6255" descrip="Reimbold & Strick fast firing opaque frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="3.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="12.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="4.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.000" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="9.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved