Frit VO 6253

Reimbold & Strick stoneware frit

OxideAnalysisFormula
BaO10.00%0.147
CaO13.00%0.521
Li2O2.00%0.151
K2O3.00%0.072
ZnO4.00%0.110
Al2O35.00%0.110
B2O36.00%0.194
SiO257.00%2.131
Oxide Weight224.69
Formula Weight224.69
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 67 x 10-7 (20-400C)
GSPT - Frit Softening Point 620C
GTTM - Glass Transition Temperature 570C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit VO 6253" descrip="Reimbold & Strick stoneware frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="10.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="13.000" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="2.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="4.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="57.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved