Frit VO 6205

Reimbold & Strick fast firing frit

OxideAnalysisFormula
CaO13.00%0.443
MgO2.00%0.095
K2O5.00%0.102
Na2O1.00%0.031
ZnO14.00%0.329
Al2O36.00%0.113
B2O33.00%0.082
SiO256.00%1.783
Oxide Weight191.37
Formula Weight191.37
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 66 X 10-7 (20-400C)
GSPT - Frit Softening Point >800C
GTTM - Glass Transition Temperature 660C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit VO 6205" descrip="Reimbold & Strick fast firing frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="13.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="14.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="3.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved