Frit VO 6200

Reimbold & Strick fast firing opaque frit

OxideAnalysisFormula
CaO8.00%0.358
MgO2.00%0.125
K2O4.00%0.107
Na2O1.00%0.041
ZnO12.00%0.370
Al2O35.00%0.123
B2O36.00%0.216
SiO253.00%2.214
ZrO29.00%0.183
Oxide Weight251.10
Formula Weight251.10
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 60 x 10-7 (20-400C)
GSPT - Frit Softening Point 790C
GTTM - Glass Transition Temperature 620C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit VO 6200" descrip="Reimbold & Strick fast firing opaque frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="8.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="12.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.000" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="9.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved