Frit VO 6170

Reimbold & Strick strontium tableware frit

OxideAnalysisFormula
BaO1.00%0.021
CaO9.00%0.520
Li2O1.00%0.109
MgO1.00%0.080
K2O3.00%0.103
Na2O2.00%0.104
SrO2.00%0.063
Al2O312.00%0.381
B2O313.00%0.605
SiO256.00%3.018
Oxide Weight323.91
Formula Weight323.91
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 59 x 10-7 (20-400C)
GSPT - Frit Softening Point 690C
GTTM - Glass Transition Temperature 610C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit VO 6170" descrip="Reimbold & Strick strontium tableware frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="1.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.000" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="1.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.000" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="2.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved