Frit VO 6160

Reimbold & Strick fast firing Zn,Ba matte frit

OxideAnalysisFormula
BaO18.00%0.267
CaO3.00%0.122
MgO1.00%0.057
K2O1.00%0.024
Na2O3.00%0.110
ZnO15.00%0.420
Al2O37.00%0.156
B2O35.00%0.164
SiO236.00%1.365
ZrO211.00%0.203
Oxide Weight227.80
Formula Weight227.80
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 56 x 10-7 (20-400C)
GSPT - Frit Softening Point 660C
GTTM - Glass Transition Temperature 600C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit VO 6160" descrip="Reimbold & Strick fast firing Zn,Ba matte frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="18.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="15.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="5.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="36.000" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="11.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved