Frit VO 6147

Reimbold & Strick fast firing Zn,Ca matte frit

OxideAnalysisFormula
CaO14.00%0.422
Na2O6.00%0.163
ZnO20.00%0.415
Al2O313.00%0.215
SiO247.00%1.321
Oxide Weight168.91
Formula Weight168.91
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 73 x 10-7 (20-400C)
GSPT - Frit Softening Point >800C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit VO 6147" descrip="Reimbold & Strick fast firing Zn,Ca matte frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="20.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="47.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved