Frit VO 6134

Reimbold & Strick frit for color development

OxideAnalysisFormula
CaO10.00%0.625
K2O4.00%0.149
Na2O4.00%0.226
Al2O313.00%0.447
B2O315.00%0.756
SiO254.00%3.150
Oxide Weight350.59
Formula Weight350.59
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 68 x 10-7 (20-400C)
GSPT - Frit Softening Point 700C
GTTM - Glass Transition Temperature 620C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit VO 6134" descrip="Reimbold & Strick frit for color development" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="15.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved