Frit VO 6104

Reimbold & Strick calcium matte frit

OxideAnalysisFormula
CaO30.00%0.917
Na2O3.00%0.083
Al2O33.00%0.050
B2O310.00%0.246
SiO254.00%1.541
Oxide Weight171.48
Formula Weight171.48
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 80 x 10-7 (20-400C)
GSPT - Frit Softening Point >800C
GTTM - Glass Transition Temperature 602C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit VO 6104" descrip="Reimbold & Strick calcium matte frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="30.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="10.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved