Frit VO 6086

Reimbold & Strick barium matte frit

OxideAnalysisFormula
BaO25.00%0.499
CaO5.00%0.273
K2O7.00%0.228
Al2O312.00%0.360
SiO251.00%2.599
Oxide Weight306.26
Formula Weight306.26
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 67 x 10-7 (20-400C)
GSPT - Frit Softening Point >800C
GTTM - Glass Transition Temperature 660C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit VO 6086" descrip="Reimbold & Strick barium matte frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="25.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="7.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved