OxideAnalysisFormula
CaO6.00%0.499
K2O1.00%0.050
Na2O6.00%0.451
Al2O37.00%0.320
B2O313.00%0.871
SiO255.00%4.270
ZrO212.00%0.454
Oxide Weight466.54
Formula Weight466.54
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 58 x 10-7 (20-400C)
GSPT - Frit Softening Point 670C
GTTM - Glass Transition Temperature 600C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit VO 6079" descrip="Reimbold & Strick opacified stoneware opaque frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.000" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="12.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved