Frit RCG 2430

Alternate Names: F RCG 2430, RCG2430, RCG-2430

OxideAnalysisFormula
CaO13.90%0.693
K2O0.60%0.018
Na2O6.40%0.289
Al2O39.70%0.266
B2O313.20%0.531
SiO256.20%2.617
Oxide Weight279.82
Formula Weight279.82
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit RCG 2430" descrip="" searchkey="F RCG 2430, RCG2430, RCG-2430" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="13.900" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.200" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved