Frit P3134

This is actually Ferro Frit 3134

Alternate Names: PotteryCrafts Frit P3134

Oxide Weight190.69
Formula Weight190.69
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.6
MLRG - Frit Melting Range (C) 980-1000C

Out Bound Links

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit P3134" descrip="This is actually Ferro Frit 3134" searchkey="PotteryCrafts Frit P3134" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="20.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.300" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="23.100" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="46.500" tolerance=""/> </oxides> </material>

Feedback, Suggestions

Your email address


Your Name


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved