Frit P2950

Lead alumina bilsilicate frit

Alternate Names: PotteryCrafts Frit 2950,PotteryCrafts Frit P2950

OxideAnalysisFormula
PbO65.95%1.000
Al2O32.55%0.085
SiO232.50%1.830
Oxide Weight341.82
Formula Weight341.82
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.5
MLRG - Frit Melting Range (C) 900-1100C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit P2950" descrip="Lead alumina bilsilicate frit" searchkey="PotteryCrafts Frit 2950,PotteryCrafts Frit P2950" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="65.950" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.550" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="32.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved