Frit NR 2

Alternate Names: Fritte NR 2, Frit NR2

OxideAnalysisFormula
CaO11.90%0.787
K2O5.40%0.213
Al2O311.80%0.429
B2O317.60%0.938
SiO253.20%3.285
Oxide Weight370.76
Formula Weight370.76
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 665 C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit NR 2" descrip="" searchkey="Fritte NR 2, Frit NR2" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.900" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="11.800" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="17.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.200" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved