Frit MOK 1

OxideAnalysisFormula
BaO2.84%0.052
CaO11.01%0.546
MgO0.45%0.031
K2O0.04%0.001
Na2O8.26%0.370
Al2O36.42%0.175
B2O316.23%0.648
SiO253.40%2.471
Oxide Weight274.33
Formula Weight274.33
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit MOK 1" descrip="" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="2.840" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.010" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.450" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.040" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.260" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.420" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="16.230" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.400" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved