Frit J

Danish frit

Alternate Names: Fritte J

OxideAnalysisFormula
CaO8.80%0.366
MgO0.02%0.001
K2O8.70%0.215
Na2O11.10%0.418
Al2O39.00%0.206
B2O313.50%0.452
SiO248.80%1.894
Oxide Weight233.05
Formula Weight233.05
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 780 C

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit J" descrip="Danish frit" searchkey="Fritte J" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="8.800" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.020" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="8.700" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="11.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved