Frit G-23

LEADED FRIT

OxideAnalysisFormula
Na2O6.46%0.282
PbO59.17%0.718
B2O314.54%0.566
SiO219.82%0.893
Oxide Weight270.72
Formula Weight270.72
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit G-23" descrip="LEADED FRIT" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.465" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="59.173" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.540" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="19.822" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved