Frit Fsb571

Leadless Borosilicate Frit

OxideAnalysisFormula
CaO9.00%0.700
MgO0.50%0.054
Na2O3.50%0.246
Al2O312.00%0.513
B2O318.00%1.128
SiO256.50%4.100
Oxide Weight433.96
Formula Weight433.96
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit Fsb571" descrip="Leadless Borosilicate Frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="18.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved