Frit Fsb510/866

High Alkaline Borosilicate Frit

OxideAnalysisFormula
CaO12.00%0.505
Na2O13.00%0.495
Al2O32.00%0.046
B2O329.00%0.984
SiO245.00%1.768
Oxide Weight238.44
Formula Weight238.44
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 1080C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit Fsb510/866" descrip="High Alkaline Borosilicate Frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="12.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="13.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="29.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="45.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved