Frit FR-170A

Opaque white glaze frit cone 06-04

OxideAnalysisFormula
BaO1.50%0.056
CaO0.60%0.061
MgO0.90%0.127
Na2O5.50%0.506
ZnO1.00%0.070
PbO7.00%0.179
Al2O35.70%0.319
B2O313.90%1.140
SiO251.50%4.892
ZrO212.40%0.574
Oxide Weight570.88
Formula Weight570.88
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit FR-170A" descrip="Opaque white glaze frit cone 06-04" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="1.500" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.600" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.900" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.500" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="1.000" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="7.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.900" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.500" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="12.400" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved