Frit A 8962

Reimbold & Strick frit for crystal glazes

OxideAnalysisFormula
Na2O16.00%1.000
Al2O337.00%1.406
SiO247.00%3.030
Oxide Weight387.50
Formula Weight387.50
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 86 x 10-7 (20-400C)
GSPT - Frit Softening Point 570C
GTTM - Glass Transition Temperature 540C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 8962" descrip="Reimbold & Strick frit for crystal glazes" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="16.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="37.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="47.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved