Frit A 62

Reimbold & Strick stoneware frit

OxideAnalysisFormula
CaO7.00%0.403
Na2O2.00%0.104
PbO34.00%0.492
Al2O36.00%0.190
B2O313.00%0.604
SiO238.00%2.044
Oxide Weight323.24
Formula Weight323.24
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 66 x 10-7 (20-400C)
GSPT - Frit Softening Point 610C
GTTM - Glass Transition Temperature 560C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 62" descrip="Reimbold & Strick stoneware frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.000" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="34.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="38.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved