Frit A 4043

Reimbold & Strick high melting frit

OxideAnalysisFormula
CaO12.00%0.562
MgO5.00%0.326
K2O4.00%0.112
Al2O311.00%0.283
SiO268.00%2.974
Oxide Weight262.86
Formula Weight262.86
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 58 x 10-7 (20-400C)
GSPT - Frit Softening Point >800C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 4043" descrip="Reimbold & Strick high melting frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="12.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="5.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="11.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="68.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved