Frit A 4040

Reimbold & Strick stoneware frit

OxideAnalysisFormula
BaO3.00%0.081
CaO3.00%0.222
MgO1.00%0.103
K2O2.00%0.088
Na2O6.00%0.402
ZnO2.00%0.102
Al2O38.00%0.326
B2O314.00%0.837
SiO261.00%4.221
Oxide Weight415.91
Formula Weight415.91
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 54 x 10-7 (20-400C)
GSPT - Frit Softening Point 640C
GTTM - Glass Transition Temperature 570C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 4040" descrip="Reimbold & Strick stoneware frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="3.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="2.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="61.000" tolerance=""/> </oxides> </material>