Frit A 4018

Reimbold & Strick fast fire high barium matte frit

OxideAnalysisFormula
BaO37.00%0.454
K2O3.00%0.060
ZnO21.00%0.486
Al2O35.00%0.092
SiO234.00%1.065
Oxide Weight188.26
Formula Weight188.26
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 105 x 10-7 (20-400C)
GSPT - Frit Softening Point >800C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 4018" descrip="Reimbold & Strick fast fire high barium matte frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="37.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="21.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="34.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved