Frit A 4015

Reimbold & Strick low melting Li frit

OxideAnalysisFormula
Li2O4.00%0.342
Na2O16.00%0.658
B2O337.00%1.355
SiO243.00%1.824
Oxide Weight254.91
Formula Weight254.91
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 96 x 10-7 (20-400C)
GSPT - Frit Softening Point 540C
GTTM - Glass Transition Temperature 500C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 4015" descrip="Reimbold & Strick low melting Li frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="4.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="16.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="37.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="43.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved