Frit A 3383

Reimbold & Strick high melting low exp matte frit

OxideAnalysisFormula
BaO3.00%0.076
CaO5.00%0.345
Li2O3.00%0.389
ZnO4.00%0.190
Al2O323.00%0.872
SiO262.00%3.991
Oxide Weight386.84
Formula Weight386.84
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 18 x 10-7 (20-400C)
GSPT - Frit Softening Point >800C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 3383" descrip="Reimbold & Strick high melting low exp matte frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="3.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.000" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="3.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="4.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="23.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="62.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved