Frit A 3382

Reimbold & Strick zero CaO stoneware frit

OxideAnalysisFormula
Na2O7.00%1.000
Al2O36.00%0.521
B2O324.00%3.054
SiO263.00%9.285
Oxide Weight885.71
Formula Weight885.71
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 49 x 10-7 (20-400C)
GSPT - Frit Softening Point 590C
GTTM - Glass Transition Temperature 520C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 3382" descrip="Reimbold & Strick zero CaO stoneware frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="24.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="63.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved