Frit A 3367

Reimbold & Strick copper frit

OxideAnalysisFormula
BaO10.00%0.394
CaO2.00%0.216
Na2O4.00%0.390
Al2O34.00%0.237
B2O315.00%1.303
SiO249.00%4.929
Oxide Weight507.86
Formula Weight507.86
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 53 x 10-7 (20-400C)
GSPT - Frit Softening Point 640C
GTTM - Glass Transition Temperature 600C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 3367" descrip="Reimbold & Strick copper frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="10.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="15.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved