Frit A 3364

Reimbold & Strick iron frit

OxideAnalysisFormula
BaO10.00%0.276
CaO3.00%0.226
Na2O5.00%0.341
ZnO3.00%0.156
Al2O38.00%0.332
B2O313.00%0.791
SiO242.00%2.959
Oxide Weight355.62
Formula Weight355.62
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 65 X 10-7 (20-400C)
GSPT - Frit Softening Point 610C
GTTM - Glass Transition Temperature 530C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 3364" descrip="Reimbold & Strick iron frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="10.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="3.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="42.000" tolerance=""/> </oxides> </material>