Frit A 3360

Reimbold & Strick barium stoneware frit

OxideAnalysisFormula
BaO7.00%0.160
CaO7.00%0.438
Li2O1.00%0.118
Na2O5.00%0.283
Al2O37.00%0.241
B2O315.00%0.757
SiO258.00%3.390
Oxide Weight351.32
Formula Weight351.32
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 60 x 10-7 (20-400C)
GSPT - Frit Softening Point 650C
GTTM - Glass Transition Temperature 590C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 3360" descrip="Reimbold & Strick barium stoneware frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="7.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.000" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="1.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="15.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="58.000" tolerance=""/> </oxides> </material>