Frit A 3334

Reimbold & Strick lead borosilicate frit

OxideAnalysisFormula
PbO55.00%1.000
B2O317.00%0.991
SiO228.00%1.891
Oxide Weight405.82
Formula Weight405.82
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 59 x 10-7 (20-400C)
GSPT - Frit Softening Point 510C
GTTM - Glass Transition Temperature 480C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 3334" descrip="Reimbold & Strick lead borosilicate frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="55.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="17.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="28.000" tolerance=""/> </oxides> </material>