Frit A 3323

Reimbold & Strick stoneware opaque frit

OxideAnalysisFormula
BaO2.00%0.052
CaO4.00%0.283
MgO2.00%0.197
K2O2.00%0.084
Na2O6.00%0.384
Al2O39.00%0.350
B2O314.00%0.798
SiO252.00%3.434
ZrO29.00%0.290
Oxide Weight396.86
Formula Weight396.86
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 58 x 10-7 (20-400C)
GSPT - Frit Softening Point 640C
GTTM - Glass Transition Temperature 560C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 3323" descrip="Reimbold & Strick stoneware opaque frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="2.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.000" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="9.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved