Frit A 3158

Reimbold & Strick low expansion low melting frit

OxideAnalysisFormula
CaO3.00%0.293
Na2O8.00%0.707
Al2O32.00%0.107
B2O336.00%2.834
SiO251.00%4.650
Oxide Weight547.92
Formula Weight547.92
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 55 x 10-7 (20-400C)
GSPT - Frit Softening Point 560C
GTTM - Glass Transition Temperature 530C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 3158" descrip="Reimbold & Strick low expansion low melting frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="36.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved