Frit A 3129

Reimbold & Strick stoneware matte frit

OxideAnalysisFormula
CaO1.00%0.033
K2O2.00%0.039
ZnO25.00%0.561
PbO45.00%0.368
Al2O33.00%0.054
SiO224.00%0.729
Oxide Weight182.55
Formula Weight182.55
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 62 x 10-7 (20-400C)
GSPT - Frit Softening Point 560C
GTTM - Glass Transition Temperature 490C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 3129" descrip="Reimbold & Strick stoneware matte frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="25.000" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="45.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="24.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved