Frit A 3128

Reimbold & Strick stoneware matte frit

OxideAnalysisFormula
BaO8.00%0.072
CaO10.00%0.245
Na2O8.00%0.177
ZnO30.00%0.506
Al2O33.00%0.040
B2O35.00%0.099
SiO236.00%0.823
Oxide Weight137.36
Formula Weight137.36
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 74 x 10-7 (20-400C)
GSPT - Frit Softening Point 610C
GTTM - Glass Transition Temperature 560C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 3128" descrip="Reimbold & Strick stoneware matte frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="8.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="30.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="5.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="36.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved