Frit A 3069

Reimbold & Strick low expansion Li frit

Alternate Names: Frit A3069

OxideAnalysisFormula
Li2O2.00%0.474
MgO3.00%0.526
Al2O39.00%0.623
B2O329.00%2.943
SiO257.00%6.700
Oxide Weight706.44
Formula Weight706.44
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 40 x 10-7 (20-400C)
GSPT - Frit Softening Point 640C
GTTM - Glass Transition Temperature 540C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 3069" descrip="Reimbold & Strick low expansion Li frit" searchkey="Frit A3069" loi="0.00" casnumber=""> <oxides> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="2.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="3.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="29.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="57.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved