Frit A 3032

Reimbold & Strick low expansion stoneware frit

Alternate Names: Frit A3032

OxideAnalysisFormula
CaO7.00%0.392
Na2O12.00%0.608
Al2O312.00%0.370
B2O37.00%0.316
SiO262.00%3.241
Oxide Weight314.14
Formula Weight314.14
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 75 x 10-7 (20-400C)
GSPT - Frit Softening Point 640C
GTTM - Glass Transition Temperature 600C

A frit manufacturer that freely publishes chemistry? Yes!

A frit manufacturer that freely publishes chemistry? Yes!

I am impressed with this Italian frit company, Reimbold & Strick. Their frit data is quite educational, by studying the chemistry of their matte frits, for example, you can see the various mechanisms that produce the effect.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 3032" descrip="Reimbold & Strick low expansion stoneware frit" searchkey="Frit A3032" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="12.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="7.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="62.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved