Frit A 3021

Reimbold & Strick low expansion Ca-B frit

Alternate Names: Frit A3021

OxideAnalysisFormula
CaO10.00%1.000
Al2O310.00%0.550
B2O326.00%2.096
SiO251.00%4.761
ZrO23.00%0.137
Oxide Weight561.00
Formula Weight561.00
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 42 X 10-7 (20-400C)
GSPT - Frit Softening Point 710C
GTTM - Glass Transition Temperature 650C

A frit manufacturer that freely publishes chemistry? Yes!

A frit manufacturer that freely publishes chemistry? Yes!

I am impressed with this Italian frit company, Reimbold & Strick. Their frit data is quite educational, by studying the chemistry of their matte frits, for example, you can see the various mechanisms that produce the effect.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 3021" descrip="Reimbold & Strick low expansion Ca-B frit" searchkey="Frit A3021" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="26.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="51.000" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="3.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved