Frit A 2912

Reimbold & Strick low solubility lead frit

OxideAnalysisFormula
PbO60.00%1.000
Al2O37.00%0.255
SiO233.00%2.043
Oxide Weight372.00
Formula Weight372.00
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 53 x 10-7 (20-400C)
GSPT - Frit Softening Point 640C
GTTM - Glass Transition Temperature 600C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 2912" descrip="Reimbold & Strick low solubility lead frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="60.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="33.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved