Frit A 2010

Reimbold & Strick low melting lead frit

OxideAnalysisFormula
Na2O6.00%0.238
PbO69.00%0.762
B2O312.00%0.425
SiO213.00%0.533
Oxide Weight246.36
Formula Weight246.36
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 111 x 10-7 (20-400C)
GSPT - Frit Softening Point 410C
GTTM - Glass Transition Temperature 380C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 2010" descrip="Reimbold & Strick low melting lead frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.000" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="69.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="13.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved