Frit A 1561

Reimbold & Strick stoneware matte frit

OxideAnalysisFormula
CaO5.00%0.136
K2O3.00%0.049
Na2O10.00%0.246
ZnO29.00%0.543
PbO4.00%0.027
Al2O33.00%0.045
B2O38.00%0.175
SiO238.00%0.963
Oxide Weight152.33
Formula Weight152.33
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 84 x 10-7 (20-400C)
GSPT - Frit Softening Point 580C
GTTM - Glass Transition Temperature 530C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Frit A 1561" descrip="Reimbold & Strick stoneware matte frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="29.000" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="4.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="8.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="38.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved